Atomic Layer Deposition of Vanadium Dioxide and a Temperature-dependent Optical Model

11.8K Views

11:10 min

May 23rd, 2018

DOI :

10.3791/57103-v

May 23rd, 2018


Przeglądaj więcej filmów

Atomic Layer Deposition

Rozdziały w tym wideo

0:04

Title

0:56

Atomic Layer Deposition (ALD) of Amorphous Vanadium Dioxide (VO2 ) on Sapphire Substrates

3:06

Annealing Amorphous VO2 Thin Films

4:45

Characterization of VO2 Films by Raman Spectroscopy

5:43

Characterization of VO2 Films by X-Ray Photoelectron Spectroscopy (XPS)

7:31

Morphological Characterization by Atomic Force Microscopy (AFM)

9:06

Results: Characterization of Amorphousand Crystalline VO2 Films

10:49

Conclusion

Powiązane Filmy

article

07:23

Construction and Testing of Coin Cells of Lithium Ion Batteries

31.3K Views

article

11:57

Fabricating Metamaterials Using the Fiber Drawing Method

13.7K Views

article

13:39

Optical Trapping of Nanoparticles

22.3K Views

article

10:27

Fabrication of Nano-engineered Transparent Conducting Oxides by Pulsed Laser Deposition

15.4K Views

article

09:40

Measurement and Analysis of Atomic Hydrogen and Diatomic Molecular AlO, C2, CN, and TiO Spectra Following Laser-induced Optical Breakdown

14.1K Views

article

14:13

Atomic Force Microscopy of Red-Light Photoreceptors Using PeakForce Quantitative Nanomechanical Property Mapping

11.7K Views

article

14:01

Making Record-efficiency SnS Solar Cells by Thermal Evaporation and Atomic Layer Deposition

42.6K Views

article

11:10

Fabrication and Operation of a Nano-Optical Conveyor Belt

11.5K Views

article

08:19

Digital Printing of Titanium Dioxide for Dye Sensitized Solar Cells

12.7K Views

article

08:38

Electrospray Deposition of Uniform Thickness Ge23Sb7S70 and As40S60 Chalcogenide Glass Films

8.4K Views

JoVE Logo

Prywatność

Warunki Korzystania

Zasady

Badania

Edukacja

O JoVE

Copyright © 2025 MyJoVE Corporation. Wszelkie prawa zastrzeżone